Preparation of ATO coating by Coating rod

Cleaning of the glass substrate: first wash with sodium hydroxide solution to remove dust , then rinse with deionized water, take it out and dry it at room temperature.

Preparation of the coating: use an  80 μm  wire Bar Coater to coat the cleaned glass slide and flat glass at a constant speed at a certain angle, and the coating will be transparent after curing under appropriate temperature and time conditions. Insulation coating . Prepare multiple samples of the same component, and take the average value of parallel tests.

Preparation of ATO coating with wire rod and coating stick Figure 1

 